Copper-Aluminum Composite PV Ribbon

PV interconnect ribbon on the cell surface
PV interconnect ribbon on the cell surface

Raytron’s copper-aluminum composite ribbon is designed for solar-module interconnection with reduced copper use. Choose the conductor section and solder coating for the cell layout and stringing process, then assess resistance, joint strength and module reliability against the existing ribbon design.

For reliability, corrosion at cut ends and module tests such as thermal cycling and damp heat, see the CCA PV ribbon reliability and corrosion guide.

On this page

Ribbon forms and reference sizes

Round ribbon connects cells along the string. Flat interconnect and busbar ribbon use separately defined width and thickness for their connection positions.

PV interconnect ribbon on the cell surface

Nominal coated round diameters

Record bare and finished diameter, solder chemistry, copper fraction basis, and the spool drawing in the order specification.

Download the technical data sheet · PDF ↓

Calculated CCA50 sizing example

Bare + radial solder
0.23 mm + 2 × 15 μm → Ø 0.26 mm
Substrate copper fraction
50 wt.% ≈ 23.19 vol.%
Solder for the calculation
Sn60Pb40
Finished resistance at 20 °C
0.576 Ω/m
Finished mass per metre
0.270785 g/m

Rev.4 reference conditions: bare section ±0.01 mm, flat width ±0.05 mm, radial solder 15 ± 5 μm. Order acceptance follows the agreed drawing and test method.

See calculation conditions →

PV ribbon · Application and purchasing

Ribbon purchasing value, grounded in module applications

Cumulative module application
>50 GW
Raytron copper-aluminum composite ribbon has been used in modules totaling more than 50 GW, including BC and TOPCon designs, according to Raytron application records as of November 2026.
Lower replaced-ribbon purchasing cost
>50%
In some Chinese module-customer projects, purchasing cost for the replaced ribbon was more than 50% lower than the previous copper-ribbon solution. The percentage covers that ribbon purchase only.
TOPCon application power difference
3 W
In a 650 W-class TOPCon application, the 0.24 mm CCA-ribbon design was 3 W below the 0.24 mm copper-ribbon reference. The guide uses 650 W / 647 W to normalize the comparison.

Construction and specification

Scroll horizontally to read all columns.

ItemSpecification
Material constructionCopper-aluminum composite conductor with a separately specified solder coating
Product formPV ribbon
Geometry for quotationState bare-metal and solder-coated thickness with tolerance for flat ribbon; use diameter for round wire
SurfaceTin or solder coating options by soldering process
PackagingSpool, traverse wound spool or customer-specified package

Factory and quality

Clad-material workshop
Clad-material workshop
Rolling equipment
Rolling equipment
Cladding process

Production checks and quality documents

Inline dimensional inspection on the production line
Inline dimensional inspection on the production line
Supplier quality review (PDF)
Supplier quality review (PDF)

CCA and copper ribbon weight and material cost comparison

Assumptions · Same rectangular substrate section and one kilometre length. Copper fraction is by volume. Densities are copper 8.96 and aluminum 2.70 g/cm³. Excludes solder coating, waste, processing and taxes. Enter prices in the same currency per kg.

  

Compare finished ribbon purchasing cost

Use the same currency, tax and delivery basis. Enter the purchase mass for the ribbon being replaced, including production losses only if they are already recorded in the purchase quantity.

From ribbon selection to the order specification

PV ribbon selection sheet (PDF)
PV ribbon selection sheet (PDF)
PV ribbon order worksheet
PV ribbon order worksheet

Choose conductor geometry and solder coating separately

The aluminum-containing core and copper layer form the conductor. The outer solder coating joins it to the cell contact. Position, resistance and mechanical duty determine the base section; cell metallization and process determine the coating.

Identify interconnect, busbar or round-wire duty, then compare a representative line and module trial. Ribbon procurement savings use the cost of the ribbon being replaced, not total module manufacturing cost.

Full PV ribbon procurement guide

Specification design factors

Drawing-defined specification

Geometry and performance

  • Width, thickness and edge geometry define a narrow flat conductor.
  • Metal layers and solder or insulation coatings perform different functions.
  • Spool format, winding tension and joining behavior connect the material to the assembly process.

Selection and processing

Specify the copper-aluminum construction separately from the solder coating. Compare the required resistance, complete module geometry, conductor mass and joining results with the copper baseline. Reduced copper use at equal size is not the same comparison as an equal-resistance design.

Material and form references

PV ribbon specifications separate the metallic conductor section from the solder coating. Cell layout, wire positioning, joining and module tests describe the intended interconnection.

Standards and product forms

Product questions

How should we choose the solder coating?

State the complete solder alloy and limits, including lead-free requirements and supporting evidence where required. Check coating coverage, joint volume, flux, cell metallization and encapsulation compatibility. Low-temperature and bismuth-containing do not mean lead-free; qualify the combination with the cells, stringer and target throughput. Read the guide section →

What should a stringing trial verify?

For the TOPCon round-CCA substitution route covered in the guide, the existing local copper-ribbon flattening operation MUST be disabled or bypassed. Equipment and process staff should confirm the actual action and record the recipe revision. With flattening off, check routing, tension, edge transition, joints, EL and power before normal production release. Validate at target throughput, including multiple reels and batches during the pilot. Read the guide section →

What module validation is needed before approval?

Use matched module builds with comparable cells, encapsulation materials and important process conditions, recording suitable settings for each ribbon. Evaluate power and reliability, including EL and I–V, thermal cycling, damp heat and relevant safety checks under agreed sequences and criteria. Record the module construction, tests, results and approved application scope. Short accelerated tests do not directly establish years of outdoor life. Read the guide section →

Is copper-clad aluminum PV ribbon reliable in solar modules?

Reliability is a module-level question, not a property of the material name. Check the copper layer, cut ends and joints, then evaluate power and reliability — including EL and I–V, thermal cycling, damp heat and relevant safety checks — on matched module builds.

CCA PV ribbon reliability and corrosion guide

Related products

Request trial spools →

Prepare your inquiry

  • Width, thickness and tolerances
  • Edge condition, burr, surface and roll dimensions
  • Core and outer-layer metals, each layer or ratio, and mass or volume basis
  • Coating alloy and thickness, soldering conditions, cell layout and spool format
  • Quantity, spool or coil format, packaging and delivery destination